MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ MEGARAD™ 2081-6LR Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: CALIBRE™ MEGARAD 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resin. When exposed to a 20% intralipid emulsion solution under strained conditions, CALIBRE™ MEGARAD 2081-6LR exhibits significant property retention compared to standard polycarbonate. It also provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (gamma or electron beam). CALIBRE™ MEGARAD 2081-6LR can reduce the color shift by 50% compared to general purpose polycarbonate resins.

Main Characteristics:

  • Improved lipid resistance
  • Stabilized for high-energy radiation
  • Tested under ISO 10993
  • Transparent
  • Contains mold release
Applications:
  • Medical applications

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.32 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 68.3 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.5 MPa50 mm/min; ASTM D638
Elongation at Break 130 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2340 MPa50 mm/min; ASTM D638
Flexural Strength 96.5 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
Flexural Modulus 2410 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 567 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Tensile Impact Strength 567 kJ/m²ASTM D1822
Dart Drop, Total Energy 89.3 J3.39 m/sec; ASTM D3763
Abrasion 45[%], Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 145 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °CUnannealed; ASTM D648
 142 °CAnnealed; ASTM D648
Vicat Softening Point 151 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 1.0 %ASTM D1003
Transmission, Visible 85 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ MEGARAD™ 2081-15 Polycarbonate Resin
Trinseo CALIBRE™ MEGARAD™ 2081-22 Polycarbonate Resin

PDWST046 / 142255

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.