MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 660.5 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D 792
Additive Loading 5.0 %Primary Additive
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5900 psiASTM D 638
Elongation at Break 4.0 - 8.0 %ASTM D 638
Tensile Modulus 330 ksiASTM D 638
Flexural Strength 10300 psiASTM D 790
Flexural Modulus 340 ksiASTM D 790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 8.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 2.0 ohm-cmASTM D 257
Surface Resistance <= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness 30 dB
@Thickness 2.00 mm,
Frequency 500000 Hz
ASTM D 4935
 31 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 32 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 32 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 32 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 33 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 475 °F
Mold Temperature 150 - 180 °F
Drying Temperature 180 °F
@Time 7200 sec
Moisture Content 0.10 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehmann & Voss LUVOCOM® 16-8960/ES Polyarylamide with carbon fiber and steel fiber
RTP Company RTP 0899 X 87096 EG BLACK Acetal (POM)
RTP Company RTP 1399X67317C Polyphenylene Sulfide (PPS), GF, Stainless Steel Fiber, EMI
RTP Company RTP 199X67314C Polypropylene, Chemically Coupled, GF, Stainless Steel Fiber, EMI
RTP Company RTP 299X67315C Nylon 6/6, GF, Stainless Steel Fiber, EMI

PQZWA2903 / 91412

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.