MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-LOY™ Compound D3000IEU6 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-LOY D3000IEU6 Compound is a static dissipative Polycarbonate Copolymer based compound that has been designed towards ATEX compliant applications. The material has an optimized balance between surface resistivity and impact strength retention after hydro aging, and has excellent low temperature impact. The material is available in a wide range of dark and light colors, including UV stabilization.

Features: Electrostatic discharge (ESD),Hydrolytic Stability,Enhanced Low Temperature Impact,Enhanced Ductility,Easy Flow,Amorphous,General Purpose,Custom Color,Appearance & Durability,Dielectrics,Thin Wall,Colorable,Color Stability,Weatherable,UV Resistant,High Impact Resistance,High Flow,Heat Stabilized,Good Moldability,Good Mold Release,Ductile,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Density 1.16 g/ccISO 1183
Water Absorption 0.70 %
@Time 86400 sec
ASTM D570
 0.70 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0300 %Injection Molding
 0.150 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium 0.30 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 3.5 %ASTM D570
 3.5 %ISO 62-1
Viscosity 5.0 cP
@Load 2.16 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
 15 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
 23 cP
@Load 5.00 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cmSABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 78.0 MPaH358/30; ISO 2039-1
Tensile Strength, Yield 45.0 MPa50 mm/min; ASTM D638
 45.0 MPa50 mm/min; ISO 527
Elongation at Break >= 60 %50 mm/min; ASTM D638
 >= 60 %50 mm/min; ASTM D638
 >= 60 %50 mm/min; ISO 527
 >= 60 %50 mm/min; ISO 527
Elongation at Yield 5.5 %50 mm/min; ASTM D638
 5.5 %50 mm/min; ISO 527
Tensile Modulus 1750 MPa50 mm/min; ASTM D638
 1750 MPa1 mm/min; ISO 527
Flexural Strength 70.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 70.0 MPa2 mm/min; ISO 178
Flexural Modulus 1825 MPa2 mm/min; ISO 178
 1900 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 850 JASTM D256
 750 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 60.0 kJ/m²80*10*4; ISO 180/1A
 65.0 kJ/m²80*10*3; ISO 180/1A
 60.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 65.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 60.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 60.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 35.0 Jpeak; ASTM D3763
 40.0 JASTM D3763
 35.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 40.0 J
@Temperature -30.0 °C
ASTM D3763
Impact Test 55.0 JMulti-Axial Instrumented Impact Energy @ peak, 23°C; ISO 6603-2
 55.0 JMulti-Axial Instrumented Impact Energy @ peak, -30°C; ISO 6603-2
 65.0 JMulti-Axial Instrumented Impact Total Energy, 23°C; ISO 6603-2
 65.0 JMulti-Axial Instrumented Impact Total Energy, -30°C; ISO 6603-2
Dart Drop Test 408000 gASTM D3763
 489600 g
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 - 1.00e+11 ohmASTM D257
 1.00e+9 - 1.00e+11 ohmROA; IEC 60093
Static Decay <= 0.010 sec5000V to <50V; FTMS101B
Dielectric Constant 2.73
@Frequency 6.00e+10 - 9.00e+10 Hz
Dissipation Factor 0.022
@Frequency 6.00e+10 - 9.00e+10 Hz
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 85.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 110 µm/m-°C
@Temperature 23.0 - 50.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 123 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 123 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 123 °CRate B/120; ASTM D1525
 123 °CRate B/50; ASTM D1525
 123 °CRate B/120; ISO 306
 123 °CRate B/50; ISO 306
 137 °CRate A/50; ISO 306
 138 °CRate A/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 260 °C
Zone 2 230 - 250 °C
Zone 3 240 - 260 °C
Melt Temperature 240 - 260 °CInjection Molding
Mold Temperature 50.0 - 90.0 °C
Drying Temperature 80.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
 
Descriptive Properties
Screw speed (Circumferential speed)0.15-0.2 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81410 / 289357

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.