Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50. Comments/Applications: Low viscosity polyamidoamine for solvent free systems. Good mechanical properties. Adhesives, sealants, flooring and coatings. Data provided by Ciba Specialty Chemicals. Ciba Specialty Chemicals has been acquired by Huntsman. |