MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 50 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce strong heat seals to polypropylene (PP). Although designed especially to seal to polypropylene, Mylar® RL43 will produce strong seals to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), and polystyrene (HIPS). Mylar® RL43 has the same type heat seal layer as Mylar® RL42, but the seal layer is thicker than Mylar® RL42. Mylar® RL43 produces the highest seal strengths to polypropylene of Mylar® lidding films and tends to produce tearing seals to non-polar substrates under chilled conditions. Mylar® RL43 is recommended when light caulking is needed. Mylar® RL43, like other RL types, has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccCalculated from nominal thickness and yield
Moisture Vapor Transmission 0.980 cc-mm/m²-24hr-atmProc. E; ASTM E96
Oxygen Transmission 3.15 cc-mm/m²-24hr-atmTested per ASTM D3985 at 22°C
Thickness 0.500 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882
Film Elongation at Break, TD 80 %ASTM D882
Secant Modulus 3.79 GPaStiffness Modulus; ASTM D882
Tear Strength Test 0.70lb Graves; ASTM D1004
Film Tensile Strength at Break, MD 172 MPaASTM D882
Film Tensile Strength at Break, TD 241 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 50 Gauge
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 50 Gauge
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 50 Gauge

PDU7E9 / 33239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.