MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baytec® OCS 080D Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec OCS 080D is a two-component polyurethane/-urea system that yields an optically clear solid elastomer.

Properties / Applications: Baytec OCS 080D is a two-component polyurethane/-urea system that yields an optically clear solid elastomer. The isocyanate component A is an aliphatic isocyanate-terminated (rMDI) polyester prepolymer, and the polyol component is a proprietary polyester formulation. The Baytec OCS 080D system can be used to produce highly transparent, optical/ballistic-grade parts for applications ranging from ophthalmic lenses to bulletproof enclosures. As with any product, the Baytec OCS 080D system must be tested (including field testing, etc) in advance by the user to determine suitability for a given application.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPolyol
 1.086 g/ccIsocyanate
 1.11 g/cc
 1.03 g/cc
@Temperature 65.0 °C
Component B
 1.036 g/cc
@Temperature 45.0 °C
Component B
 1.044 g/cc
@Temperature 25.0 °C
Component B
 1.074 g/cc
@Temperature 65.0 °C
Component A
 1.082 g/cc
@Temperature 35.0 °C
Component A
 1.086 g/cc
@Temperature 25.0 °C
Component A
Viscosity 680 cPPolyol
 1378 cPIsocyanate
 50 cP
@Temperature 65.0 °C
Component A
 100 cP
@Temperature 65.0 °C
Component B
 250 cP
@Temperature 35.0 °C
Component A
 550 cP
@Temperature 35.0 °C
Component B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
Tensile Strength at Break 59.5 MPa
Flexural Modulus 1720 MPa
Izod Impact, Notched 1.31 ft-lb/in
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 154.6 °C
Flash Point >= 93.0 °CIsocyanate
 >= 93.0 °CPolyol
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
Haze <= 0.50 %
Transmission, Visible 92 %
 
Processing PropertiesOriginal ValueComments
Mold Temperature 110 °C
 
Descriptive Properties
AppearanceColorless to pale yellow liquidIsocyanate
 Yellow liquidPolyol
Content19.6-20.3%NCO, Isocyanate
 420-432[mg KOH/g], OH Number, Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® TTX163 + MOCA, 95 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX174 + MOCA, 60 D Polyurethane, TDI- PTMEG
Covestro Baydur® GS PIR A Polyurethane
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TT174 + BAYTEC® XL 1705, 58 D Polyurethane, TDI- PTMEG

PCOVEST0258 / 202041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.