MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics Luminex™ 993 Mac-MO995S Technical Ceramic
Categories: Ceramic

Material Notes: A very high-purity porous magnesia ceramic.

Applications:

  • Special cabling for control systems in nuclear power stations where low neutron capture is of vital importance
  • Thermal processing equipment
  • Electrical control devices in industrial plant
  • Crushable bushes for electrical insulation at high temperature.

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 - 2.50 g/cc0.0795 - 0.0903 lb/in³tailorable
Porosity 28 - 38 %28 - 38 %tailorable, open
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 170 GPa
@Temperature 20.0 °C
24700 ksi
@Temperature 68.0 °F
Compressive Strength 12.0 - 170 MPa1740 - 24700 psitailorable
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  6.30e+7 ohm-cm
@Temperature 900 °C
6.30e+7 ohm-cm
@Temperature 1650 °F
 4.80e+8 ohm-cm
@Temperature 800 °C
4.80e+8 ohm-cm
@Temperature 1470 °F
 5.70e+9 ohm-cm
@Temperature 700 °C
5.70e+9 ohm-cm
@Temperature 1290 °F
 1.20e+11 ohm-cm
@Temperature 600 °C
1.20e+11 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.7 µm/m-°C
@Temperature 200 - 500 °C
6.50 µin/in-°F
@Temperature 392 - 932 °F
 13.0 µm/m-°C
@Temperature 20.0 - 1000 °C
7.22 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 8.00 - 32.0 W/m-K
@Temperature 20.0 - 900 °C
55.5 - 222 BTU-in/hr-ft²-°F
@Temperature 68.0 - 1650 °F
Maximum Service Temperature, Air 1200 °C2190 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 <= 0.050 %<= 0.050 %
CaO 0.25 %0.25 %
Fe2O3 0.070 %0.070 %
MgO 99.45 %99.45 %
Other 0.0010 %0.0010 %B +Cd
SiO2 0.19 %0.19 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
McDanel Advanced Ceramics MV-30 Mullite
Imerys HARRP™ 40 Wollastonite
CoorsTek Porcelain
CeramTec 701 Cordierite
Anderman Ceramics EM60 Mullite

CMORF8083 / 203560

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.