MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo PULSE™ 1370 ABS + Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM Data
Water Absorption 0.15 %
Moisture Absorption at Equilibrium 0.32 %Humidity Absorption
Linear Mold Shrinkage 0.0070 cm/cm
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115
Tensile Strength, Ultimate 44.8 MPaASTM Data
Tensile Strength, Yield 51.7 MPaASTM Data
Elongation at Break 125 %ASTM Data
Elongation at Yield 4.0 %ISO Data
Tensile Modulus 2.30 GPaISO Data.
Izod Impact, Notched 6.41 J/cmASTM Data
 5.34 J/cm
@Temperature -50.0 °C
ASTM Data
Charpy Impact Unnotched NBISO Data
 NBISO Data, Low Temp
Charpy Impact, Notched 2.50 J/cm²ISO Data, Low Temp
 6.60 J/cm²ISO Data
Instrumented Impact Total Energy 62.2 J
@Temperature -30.0 °C
 62.2 J
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 110 °CUnannealed; ASTM Data
 121 °Cannealed; ASTM Data
Vicat Softening Point 140 °C
Flammability, UL94 HB
@Thickness 1.47 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® WP-1069 PC/ABS, Unreinforced
Lotte Advanced Materials Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade
Lotte Advanced Materials Infino® HP-1000XA PC/ABS, Unreinforced
LG Chemical LUPOY MP5000AM PC/ABS
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact

PZZDW124 / 34355

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.