MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Dow™ 611A LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description:
  • A shrink film resin with good optics for packaging applications
  • Optimum gauge range: 1.0-3.0 mil

Complies with: US FDA 21 CFR 177.1520©2.2a; EU NO 10/2011; FDA DMF; Canadian HPFB No Objections (with limitations). Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA 21 CFR 177.1520©2.2; EU NO 10/2011; DMF; Canadian HPFB No Objections

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792
Melt Flow 0.88 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1710 psi
@Thickness 0.0508 mm
ASTM D882
 1730 psi
@Thickness 0.0254 mm
ASTM D882
Film Tensile Strength at Yield, TD 1770 psi
@Thickness 0.0508 mm
ASTM D882
 1780 psi
@Thickness 0.0254 mm
ASTM D882
Film Elongation at Break, MD 270 %
@Thickness 0.0254 mm
ASTM D882
 370 %
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, TD 540 %
@Thickness 0.0254 mm
ASTM D882
 560 %
@Thickness 0.0508 mm
ASTM D882
2% Secant Modulus 28600 psi
@Thickness 0.0254 mm
MD; ASTM D882
 29200 psi
@Thickness 0.0508 mm
MD; ASTM D882
 32600 psi
@Thickness 0.0254 mm
TD; ASTM D882
 32900 psi
@Thickness 0.0508 mm
TD; ASTM D882
Elmendorf Tear Strength MD 190 g
@Thickness 0.0254 mm
ASTM D1922
 400 g
@Thickness 0.0508 mm
ASTM D1922
Elmendorf Tear Strength TD 180 g
@Thickness 0.0254 mm
ASTM D1922
 450 g
@Thickness 0.0508 mm
ASTM D1922
Dart Drop Test 78.0 g
@Thickness 0.0254 mm
ASTM D1709A
 120 g
@Thickness 0.0508 mm
ASTM D1709A
Film Tensile Strength at Break, MD 3130 psi
@Thickness 0.0508 mm
ASTM D882
 3680 psi
@Thickness 0.0254 mm
ASTM D882
Film Tensile Strength at Break, TD 2450 psi
@Thickness 0.0508 mm
ASTM D882
 2510 psi
@Thickness 0.0254 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 234 °F
Vicat Softening Point 207 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %
@Thickness 0.0254 mm
ASTM D1003
 7.0 %
@Thickness 0.0508 mm
ASTM D1003
Gloss 71 %
@Thickness 0.0254 mm
45°; ASTM D2457
 76 %
@Thickness 0.0508 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 416 °FExtrusion
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Toughness666 ft-lb/in3MD, 1.0 mil, ASTM D882
 770 ft-lb/in3TD, 1.0 mil, ASTM D882
 780 ft-lb/in3MD, 2.0 mil, ASTM D882
 808 ft-lb/in3TD, 2.0 mil, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF469 / 311162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.