MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bayshore Vinyl Compounds BRC R409004/GP.UV Extrusion Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: BRC R409004/GP.UV is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. R409004/GP.UV has been formulated for UV resistance for interior applications where color change is a concern.

Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84ASTM D2240
Tensile Strength at Break 6600 psiASTM D638
Tensile Modulus 345 ksiASTM D638
Flexural Yield Strength 12.7 ksiASTM D790
Flexural Modulus 384 ksiASTM D790
Impact 3.9Gardner [in-lb/mil]; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 68.0 °CASTM D648
 
Descriptive Properties
Equilibrium Torque (metergrams)1850187°C, 65g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bayshore Vinyl Compounds BVC 6200-65 Vinyl Compound
Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound
Fainplast Compounds PM 50/C Flexible PVC, Extrusion
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound

PBAYS014 / 93286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.