MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.

Application examples: flexible molding, handles, closures, household items, toys, various containers (basins, buckets ...), master-batches.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.918 g/cc0.918 g/ccISO 1183
Linear Mold Shrinkage 0.020 - 0.040 cm/cm0.020 - 0.040 in/in
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
22 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151after 15 sec; ISO 868
Tensile Strength at Break 8.00 MPa1160 psiISO 527-2
Tensile Strength, Yield 8.00 MPa1160 psiISO 527-2
Elongation at Break 250 %250 %ISO 527-2
Modulus of Elasticity 0.160 GPa23.2 ksiISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 106 °C223 °FISO 11357
Vicat Softening Point 85.0 °C185 °FISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 240 °C320 - 464 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® M15HP POM, Unfilled
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded

PTOTAL711 / 130436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.