MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExOne 316L Stainless Steel for 3D Printing
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes:

Information provided by ExOne™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.60 - 7.90 g/cc
Porosity 1.00 - 4.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 67.0 - 71.0ASTM E18
Tensile Strength, Ultimate 450 - 520 MPaZ; ASTM E8
 450 - 580 MPaX & Y; ASTM E8
Tensile Strength, Yield 140 - 220 MPa
@Strain 0.2 %
X & Y; ASTM E8
 140 - 220 MPa
@Strain 0.2 %
Z; ASTM E8
Elongation at Break 40.0 - 50.0 %Z; ASTM E8
 40.0 - 55.0 %X & Y; ASTM E8
Modulus of Elasticity 180 - 190 GPaZ; ASTM E8
 190 - 220 GPaX & Y; ASTM E8
Poissons Ratio 0.280 - 0.300
Impact Test 55.0 - 75.0 JASTM E23
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.0300 %
Chromium, Cr 16.0 - 18.0 %
Iron, Fe 62.0 - 72.0 %balance
Manganese, Mn <= 2.00 %
Molybdenum, Mo 2.00 - 3.00 %
Nickel, Ni 10.0 - 14.0 %
Silicon, Si <= 1.00 %
 
Descriptive Properties
Surface Roughness3 - 12 µm Ra

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NEXONE992 / 323297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.