HCG2520MP is high rigidity and balance tenacity 20% GF PC resin. It has excellent surface, high NCVM rate, easy to machining, high stability and super shape resistance property. HCG2520MP is mainly used in mobile phone housingInformation provided by Shanghai Kumho Sunny Plastics co, Ltd |