MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 799 X 144699 A EG High Density Polyethylene (HDPE); ESD Protection - Permanently Static Dissipative - Extrusion Grade - Mineral - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D 792
Melt Flow <= 0.50 g/10 min
@Load 2.16 kg
<= 0.50 g/10 min
@Load 4.76 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262instantaneous; ASTM D 2240
Tensile Strength at Break 17.9 MPa2600 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 0.414 GPa60.0 ksiASTM D 638
Flexural Strength 17.2 MPa2500 psiASTM D 790
Flexural Modulus 0.552 GPa80.0 ksiASTM D 790
Izod Impact, Notched 1.28 J/cm
@Thickness 3.20 mm
2.40 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 1.00e+9 ohm-cm1.00e+7 - 1.00e+9 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+8 - 1.00e+10 ohm1.00e+8 - 1.00e+10 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 216 °C360 - 420 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 699 X 144695 A EG Acrylonitrile Butadiene Styrene (ABS); ESD Protection - Permanently Static Dissipative - Mineral - Extrusion Grade - Preliminary Datasheet
Polykemi AB POLYfill PP EIP5025 F VT2 Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
LNP ULTEM® SMU5831 Polyetherimide, 30% Carbon\Glass\Mineral Reinforced

PQZRA37385 / 205889

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.