System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Evonik DYNAPOL® S 1401 Linear Copolyester
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
Material Notes:
A saturated, linear copolyester, slightly crystalline. Generally used in a solution, film or melt from heated tanks or extruders for the adhesion of aluminum, PET, PVC, ABS, copper, paper, cardboard, leather and fabric
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
DIN 53 479
Viscosity
15000
cP
@Temperature 220 °C
15000
cP
@Temperature 428 °F
melt; (Plate/Plate)
25000
cP
@Temperature 200 °C
25000
cP
@Temperature 392 °F
melt; (Plate/Plate)
40000
cP
@Temperature 180 °C
40000
cP
@Temperature 356 °F
melt; (Plate/Plate)
80000
cP
@Temperature 160 °C
80000
cP
@Temperature 320 °F
melt; (Plate/Plate)
Viscosity Test
75
-
85
cm³/g
0.75
-
0.85
dl/g
DIN 53 728
Melt Flow
110
g/10 min
@Temperature 160 °C
110
g/10 min
@Temperature 320 °F
DIN ISO 1133
190
g/10 min
@Temperature 180 °C
190
g/10 min
@Temperature 356 °F
DIN ISO 1133
290
g/10 min
@Temperature 200 °C
290
g/10 min
@Temperature 392 °F
DIN ISO 1133
Chemical Properties
Metric
English
Comments
Total Acid Number
<= 3.0
<= 3.0
DIN EN ISO 2114
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
19
19
Tensile Strength, Ultimate
5.00
MPa
725
psi
DIN EN ISO 527-1/3
Elongation at Break
800 %
800 %
Thermal Properties
Metric
English
Comments
Melting Point
80.0
-
95.0
°C
176
-
203
°F
optical; Mettler FP 82
Softening Point
100
°C
212
°F
DIN ISO 4625
Glass Transition Temp, Tg
-25.0
°C
-13.0
°F
DIN 53 765
Descriptive Properties
Hydroxyl Number (mg KOH/g)
4-10
DIN 53 240-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1655E Copolyester Hotmelt Adhesive (Technical Applications)
PHUMB267 / 81269
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.