MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inovyn 386NB Polyvinyl Chloride Low Viscosity Paste
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: Made by emulsion polymerization for plastisol preparation.

MAIN APPLICATION
Spread coating :

- flooring top coat.
ADVANTAGES
- Matt appearance in flooring to coat.
- Good viscosity stability on storage.

Information provided by SolVin.

SolVin is a predecessor company to Inovyn.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content <= 0.30 g/lISO 1269
Particle Size 125 µm<0.15 g/kg greater than value; ISO 787-18
Viscosity Measurement 86K value; ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 376NB Polyvinyl Chloride Low Viscosity Paste
Inovyn 367NK Polyvinyl Chloride Medium Viscosity Paste
Inovyn 370HD Polyvinyl Chloride High Viscosity Paste
Inovyn Vinidur® 464SZ Polyvinyl Chloride grafted copolymer
Inovyn 367NF Polyvinyl Chloride Low Viscosity Paste

PSOLVI41 / 68401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.