MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin exhibit good tensile and puncture resistance properties.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Blown Film
  • Diaper Backsheet
  • Overwrap Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.2 MPa2500 psiASTM D882
Film Tensile Strength at Yield, TD 22.8 MPa3300 psiASTM D882
Film Elongation at Break, MD 770 %770 %ASTM D882
Film Elongation at Break, TD 930 %930 %ASTM D882
Puncture Energy 0.395 J0.292 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 20 g20 gASTM D1922
Elmendorf Tear Strength TD 110 g110 gASTM D1922
Dart Drop Test <= 50.0 g<= 0.110 lbASTM D1709A
Film Tensile Strength at Break, MD 49.0 MPa7100 psiASTM D882
Film Tensile Strength at Break, TD 41.4 MPa6000 psiASTM D882
1% Secant Modulus, MD 545 MPa79000 psiASTM D882
1% Secant Modulus, TD 689 MPa100000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 128 °C<= 263 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 18 %18 %ASTM D1003
Gloss 40 %40 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force5 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HF3712 Extrusion Linear Low Density Polyethylene
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1004YB Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin

PEX99162 / 175398

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.