MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® HD 50 Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® HD 50 is an ion exchange resin loaded with nutrient substances which are necessary for the nourishment of plants, mainly nitrogen, phosphorus and potassium. Lewatit HD 50 is an NPK fertilizer base on ion exchange resin with a long-term effect. It is particularly suited for the continuous nourishment of soil-less cultures of ornamental plants (hydroculture). It is in compliance with the German Fertilizer Decree 2002. It is completely insoluble in water, yet ensures a healthy growth of plants by means of the follow exchange processes. Only some of the salts contained in water, such as calcium and magnesium sulfates, are useful for the nourishment of plants. The large majority of these salts, however, cannot be utilized by the plant, and salts may even be harmful. Lewatit HD 50 adsorbs these non-useful salts and in return, to release nutrient substances into the water. Lewatit HD 50 removes e.g. common salts or calcium carbonate from the water and release e.g. ammonium nitrate or potassium phosphate in return. In the same way, Lewatit HD 50 also provides important trace elements, e.g. iron, manganese, copper, zinc, boron and molybdenum in a ready-to-use form. No matter how large an amount of Lewatit HD 50 is, that has been added to the water, the concentration of salts will not increase. While the salts without nutrient value for the plant contained in the water migrate into the water insoluble ion exchange resin, the corresponding amount of nutrient salts is released into solution. The main advantage of Lewatit HD 50 is that it continuously releases nutrient salts into the water. This release is according to the consumption of the plant. This product thus offers a much wider range of uses than liquid fertilizers for optimum nourishment of plants. According to our experience, 20-30 ml Lewatit HD 50 per 0.5 meter of each plant height is sufficient to ensure complete nourishment fo r3-4 months. The water which evaporates simply needs to be refilled. After 3-4 months, another 20-30 ml of Lewatit HD 50 should be added with the irrigation water to ensure nourishment of the plan for another 3-4 months.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.320 - 0.420 g/ccdry
 0.680 - 0.780 g/ccwet
pH 4.5 - 6.5
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 50 %
Nitrogen, N 2.0 %
P2O5 1.0 %
Potassium, K 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trimay® Wear Plate T170 Nickel-based Steel Overlay
Sandvik Sanicro 59 Covered electrodes
Sandvik Sanicro 56 Covered electrodes (UNS N10276)
Sandvik Sanicro 54 Welding wire
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded

PLANY8746 / 209139

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.