Physical Properties | Metric | English | Comments |
---|
Density | 10.2 g/cc | 0.368 lb/inĀ³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Vickers | <= 200 @Load 10.0 kg | <= 200 @Load 22.0 lb |
| 205 - 240 @Load 10.0 kg, Diameter 73.03 - 88.9 mm | 205 - 240 @Load 22.0 lb, Diameter 2.875 - 3.50 in |
| 210 - 250 @Load 10.0 kg, Diameter 47.63 - 73.03 mm | 210 - 250 @Load 22.0 lb, Diameter 1.875 - 2.875 in |
| 215 - 260 @Load 10.0 kg, Diameter 28.57 - 47.63 mm | 215 - 260 @Load 22.0 lb, Diameter 1.125 - 1.875 in |
| 225 - 270 @Load 10.0 kg, Diameter 22.2 - 28.57 mm | 225 - 270 @Load 22.0 lb, Diameter 0.875 - 1.125 in |
| 230 - 280 @Load 10.0 kg, Diameter 3.17 - 22.2 mm | 230 - 280 @Load 22.0 lb, Diameter 0.125 - 0.875 in |
Tensile Strength | >= 448 MPa @Diameter 73.03 - 88.9 mm | >= 65000 psi @Diameter 2.875 - 3.50 in |
| >= 483 MPa @Diameter 47.63 - 73.03 mm | >= 70000 psi @Diameter 1.875 - 2.875 in |
| >= 517 MPa @Diameter 3.17 - 10.319 mm | >= 75000 psi @Diameter 0.125 - 0.40625 in |
| >= 517 MPa @Diameter 28.57 - 47.63 mm | >= 75000 psi @Diameter 1.125 - 1.875 in |
| >= 586 MPa @Diameter 22.2 - 28.57 mm | >= 85000 psi @Diameter 0.875 - 1.125 in |
| >= 621 MPa @Diameter 10.319 - 22.2 mm | >= 90000 psi @Diameter 0.40625 - 0.875 in |
Tensile Strength, Yield | >= 379 MPa @Diameter 3.17 - 10.319 mm, Strain 0.2 % | >= 55000 psi @Diameter 0.125 - 0.40625 in, Strain 0.2 % |
| >= 379 MPa @Diameter 73.03 - 88.9 mm, Strain 0.2 % | >= 55000 psi @Diameter 2.875 - 3.50 in, Strain 0.2 % |
| >= 414 MPa @Diameter 47.63 - 73.03 mm, Strain 0.2 % | >= 60000 psi @Diameter 1.875 - 2.875 in, Strain 0.2 % |
| >= 448 MPa @Diameter 28.57 - 47.63 mm, Strain 0.2 % | >= 65000 psi @Diameter 1.125 - 1.875 in, Strain 0.2 % |
| >= 483 MPa @Diameter 22.2 - 28.57 mm, Strain 0.2 % | >= 70000 psi @Diameter 0.875 - 1.125 in, Strain 0.2 % |
| >= 517 MPa @Diameter 10.319 - 22.2 mm, Strain 0.2 % | >= 75000 psi @Diameter 0.40625 - 0.875 in, Strain 0.2 % |
Elongation at Break | >= 10 % @Diameter 28.57 - 47.63 mm | >= 10 % @Diameter 1.125 - 1.875 in |
| >= 10 % @Diameter 47.63 - 73.03 mm | >= 10 % @Diameter 1.875 - 2.875 in |
| >= 10 % @Diameter 73.03 - 88.9 mm | >= 10 % @Diameter 2.875 - 3.50 in |
| >= 15 % @Diameter 3.17 - 10.319 mm | >= 15 % @Diameter 0.125 - 0.40625 in |
| >= 15 % @Diameter 10.319 - 22.2 mm | >= 15 % @Diameter 0.40625 - 0.875 in |
| >= 15 % @Diameter 22.2 - 28.57 mm | >= 15 % @Diameter 0.875 - 1.125 in |
|
Component Elements Properties | Metric | English | Comments |
---|
Carbon, C | <= 0.030 % | <= 0.030 % |
Iron, Fe | <= 0.010 % | <= 0.010 % |
Molybdenum, Mo | >= 99.95 % | >= 99.95 % |
Nickel, Ni | <= 0.0020 % | <= 0.0020 % |
Nitrogen, N | <= 0.0020 % | <= 0.0020 % |
Oxygen, O | <= 0.0015 % | <= 0.0015 % |
Silicon, Si | <= 0.010 % | <= 0.010 % |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.