MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded; Acrylic, Optical Grade, Molded

Material Notes: Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are available.

Information provided by Plaskolite West, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D-955
Melt Flow 2.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 9800 psiASTM D-638
Elongation at Break 3.4 %ASTM D-638
Modulus of Elasticity 440 ksiASTM D-638
Flexural Strength 17.1 ksiASTM D-790
Izod Impact, Notched 0.350 ft-lb/in
@Thickness 6.35 mm
ASTM D-256
Gardner Impact 2.00 in-lb
@Thickness 3.17 mm
Falling Weight; ASTM D-3029 GB
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CASTM D-696
Maximum Service Temperature, Air 90.0 °CUL-746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 204 °FASTM D-648
Vicat Softening Point 216 °FASTM D-1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D-1003
Transmission, Visible 92 %ASTM D-1003
 
Descriptive Properties
3-Year WeatheringListedSAE J 576 (AMECA)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA-61 General Purpose Acrylic Resin
Plaskolite West Optix® CA-51 General Purpose Acrylic Resin
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin
Plaskolite West Optix® CA-71 General Purpose Acrylic Resin
Plaskolite West Optix® CA-82 General Purpose Acrylic Resin

PCONT038 / 150595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.