MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® 50 OL2 Polyester Film, 50 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

An exceptionally strong Mylar® polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. The film has an extra heavy heat-seal layer, which produces excellent seals to CPET trays. It also seals to ovenable, polyester coated paperboard trays. While it produces good seals, it can be stripped from the tray, before or after heating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccAverage value for Mylar® films.
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 44.0 g/m²/dayASTM E96 Procedure E
Oxygen Transmission 17.9 cc-mm/m²-24hr-atmor 1375 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 0.500 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 125 %ASTM D882
Film Elongation at Break, TD 95 %ASTM D882
Modulus of Elasticity 3.79 GPa(stiffness), ASTM D882
Tear Strength Test 350Graves, g; ASTM D1004
Seal Strength 544 g/25 mm
Film Tensile Strength at Break, MD 165 MPaASTM D882
Film Tensile Strength at Break, TD 214 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CFoods can be heated or cooked up to this temperature.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge
Westlake EC 475 Low Density Polyethylene
NatureWorks® Ingeo™ 4032D Film Grade PLA
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin
ExxonMobil Exxtra™ Seal POP 229 Plastomer for Cast Film

PDU651 / 33100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.