MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek MTEK 31 UNS R30031 Cobalt Base Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Non-galling, heat and thermal shock resistance. Heat Resistance.

Applications: Bearings and hot work sleeves, housings. Rocket engine parts

Information provided by MetalTek

Key Words: Cast UNS R30031; AMS 5382 (Investment Casting)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/ccBased on UNS number
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.45 - 0.55 %
Chromium, Cr 24.5 - 26.5 %
Cobalt, Co 49.45 - 58.55 %As Balance
Iron, Fe <= 2.0 %
Manganese, Mn <= 1.0 %
Nickel, Ni 9.5 - 11.5 %
Silicon, Si <= 1.0 %
Tungsten, W 7.0 - 8.0 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 205°C (400°F) temper, 25 mm (1 in.) round
Latrobe LSS™ 4140 Alloy Steel (AISI 4140)
Special Metals INCONEL® Alloy 718

NMETEK146 / 18396

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.