MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Data provided by the manufacturer, Owens Corning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D792
Water Absorption 0.14 %0.14 %24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ASTM D785
Tensile Strength, Ultimate 83.0 MPa12000 psiASTM D638
Elongation at Break 9.0 %9.0 %ASTM D638
Modulus of Elasticity 5.20 GPa754 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 4.00 GPa580 ksiASTM D790
Compressive Strength 97.0 MPa14100 psiASTM D695
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 60 Hz
3.1
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Arc Resistance 125 sec125 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.24 µm/m-°C
@Temperature 20.0 °C
1.80 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.21 J/g-°C0.290 BTU/lb-°F
Thermal Conductivity 0.663 W/m-K4.60 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 141 °C285 °FASTM D648
Flammability, UL94 V-1V-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
Mitsubishi Iupilon® CFH 2020 Polycarbonate
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber

POC015 / 55593

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.