MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silres® BS 17040 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® BS 17040 is a water-thinnable, solventless silane emulsion. SILRES® BS 17040 serves as highquality water repellent for impregnating and priming of alkaline mineral surfaces. Moreover SILRES® BS 17040 can be used as water resisting admixtures for non-load bearing manufactured concrete products.

Special features: SILRES® BS 17040 is characterised by:

  • good depth of penetration
  • dilutable with water, and free of solvents
  • low volatility
  • high resistance to alkalis
  • stable in storage, even when diluted treated concrete will have the following permanent properties:
  • dramatic reduction in chloride and water absorption
  • no loss in breathability
  • improved durability against freeze-thaw de-icing salt stress
  • enhanced durability
  • provides good adhesion for paints
In the construction material, SILRES® BS 17040 reacts with atmospheric moisture and / or the water in the building material’s pores, eliminating alcohol. The active thus substance formed greatly reduces the concrete’s absorbency in the active zone (penetration depth after post treatment), but without blocking any pores or capillaries. The impregnated building material retains very high water-vapor permeability.

Application: SILRES® BS 17040 is recommended for the hydrophobic impregnation and priming of concrete and reinforced concrete in road, bridge and building construction as well as water resisting admixtures for non-load bearing manufactured concrete products. For the hydrophobic impregnation of high-grade, load bearing concrete SILRES® BS 17040 must be used undiluted, as the product has been approved in that concentration according to EN 1504-2.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/cc
Volatile Organic Compounds (VOC) Content <= 350 g/lASTM D 5095-91
 
Descriptive Properties
Active ingredients (%)40
Appearancemilky, white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9560 / 205089

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.