MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ITW Irathane Futura® ULTRACHROME 452 Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A single component water based aliphatic urethane which can be used as either an in mold or post finish coating. As a post finish for speaker coatings done with Ultrathane 5410. As a post finish for other Irathane Futura systems where a UV stable finish is required.

FEATURES: • Simple to apply and fast drying • Excellent color retention • Low VOC’s.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 1.04 g/cc>= 0.0376 lb/in³
Solids Content 33 - 37 %33 - 37 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 7570 - 75ASTM D2240
Tensile Strength 18.0 - 20.0 MPa2610 - 2900 psiASTM D412
Elongation at Break 130 - 150 %130 - 150 %ASTM D412
Izod Impact Resistance 4.30 J/cm²20.5 ft-lb/in²ISO 180
Gardner Impact 5.02 J3.70 ft-lbASTM D2795
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °FTemperature Resistance
Flash Point 65.0 °C149 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 60.0 min60.0 minafter Ultrachrome 1552 addition
Shelf Life 12.0 Month
@Temperature 22.0 °C
12.0 Month
@Temperature 71.6 °F
In original unopened container in dry environment.
 
Descriptive Properties
ColorBlack
Coverage7m2 /L/50 microns dft
Mix Ratio by volume10:1452: Ultrachrome 1552
Recommended DFT25 to 50 microns1 or 2 coats

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWI9235 / 239744

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.