MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® CP-13235 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-13235 is a high performance thermoplastic elastomer that is designed for a variety of consumer product applications. Monprene CP-13235 is a low hardness, low density, high flow grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Processability; High Flow; Low Hardness; Low Density; Low Specific Gravity; Lubricated; Slip; Without Fillers

Uses: Consumer Applications; Flexible Grips; Gaskets; General Purpose; Grommets; Handles; Knobs; O-rings; Overmolding; Plug; Rubber Replacement; Seals; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  35
@Time 5.00 sec
35
@Time 0.00139 hour
Injection Molded; ASTM D2240
 37
@Time 1.00 sec
37
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 7.58 MPa1100 psiASTM D412
Elongation at Break 700 %700 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 227 °C340 - 440 °F
Middle Barrel Temperature 171 - 227 °C340 - 440 °F
Front Barrel Temperature 171 - 227 °C340 - 440 °F
Nozzle Temperature 171 - 227 °C340 - 440 °F
Melt Temperature 171 - 227 °C340 - 440 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0780 / 237271

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.