Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for processing by injection molding. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins. Data provided by the manufacturer. This former DuPont product line is now a Dow product line. |
Ethylene/Methacrylic Acid (E/MAA) Copolymer |