MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperature

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D-792
Filler Content 20 %20 %Glass
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D-955
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D-785
Tensile Strength, Yield 61.8 MPa
@Thickness 3.20 mm
8960 psi
@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Flexural Yield Strength 88.3 MPa
@Thickness 6.40 mm
12800 psi
@Thickness 0.252 in
ASTM D-790
Flexural Modulus 4.12 GPa
@Thickness 6.40 mm
597 ksi
@Thickness 0.252 in
ASTM D-790
Izod Impact, Notched  0.588 J/cm
@Thickness 6.40 mm
1.10 ft-lb/in
@Thickness 0.252 in
ASTM D-256
 0.686 J/cm
@Thickness 3.20 mm
1.29 ft-lb/in
@Thickness 0.126 in
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FMethod A - Annealed; ASTM D-648
Vicat Softening Point 115 °C239 °FMethod B; ASTM D-1525
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
UL-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBHANS40 / 27149

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.