MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This product does not contain the flame retardants mentioned in the WEEE directive (PBB or PBDE). The product is used widely throughout the electrical and appliance industries for applications like pressure switches, circuit breaker housings, contactors, timers and programmers.

Key characteristics:

  • UL listed V0 at 3.0 and 0.75 mm
  • UL listed GWIT 825 °C and GWFI 960°C at 0.75 mm, compliant with IEC 60335-4
  • UL listed on CTI PCL 1 (CTI = 425 V)
  • Excellent mechanical performance
  • Colorable in light colors
  • Easy processing

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccASTM D792, ISO 1183
Water Absorption 1.3 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 5.0 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmEuronil
Linear Mold Shrinkage, Transverse 0.0050 cm/cmEuronil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 130 MPaISO 527, ASTM D638
Elongation at Break 2.0 %ISO 527, ASTM D638
Tensile Modulus 8.00 GPaISO 527, ASTM D638
Flexural Yield Strength 190 MPaISO 178, ASTM D790
Flexural Modulus 8.60 GPaISO 178, ASTM D790
 4.20 GPa
@Temperature 90.0 °C
ISO 178, ASTM D790
Izod Impact, Notched (ISO) 6.50 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 2.80 J/cm²ISO 179
 2.00 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.800 J/cm²ISO 179
 0.600 J/cm²
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Comparative Tracking Index 275 V
@Thickness 3.20 mm
Sol. B; IEC 112, UL 746A
 425 V
@Thickness 3.20 mm
Sol. A; IEC 112, UL 746A
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 192 °CISO 75, ASTM D648
Vicat Softening Point 190 °C49 N; ISO 306, ASTM D1525
 210 °C9.8 N; ISO 306, ASTM D1525
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 0.800 mm
 V-0
@Thickness 3.20 mm
Oxygen Index 33 %ASTM D2863
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 694-2-12
 960 °C
@Thickness 3.20 mm
IEC 694-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 473 - 527 °F
Zone 1 464 - 500 °Fhopper
Zone 2 464 - 509 °F
Zone 3 464 - 518 °F
Zone 4 473 - 527 °F
Melt Temperature 250 - 270 °CDo not melt above 280°C
Mold Temperature 90.0 - 110 °CPreferred
Drying Temperature 80.0 - 85.0 °C
Dry Time 4 hour
Injection Pressure 70.0 - 100 MPa
 
Descriptive Properties
Clamping Forcein tons, 0.7 times the projected surface area in cm2
Flammability RatingSEFMVSS No. 302, 355x100x1 mm
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Holding Pressure90 MPa
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA® H130 30% Glass Filled Liquid Crystal Polymer (LCP)
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Covestro Bayblend® FR3010 HF PC/ABS Blend
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced

PLBN56 / 50445

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.