MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typical applications include transformer spacers and supports. A NEMA GPO-1 grade fiberglass mat reinforced thermoset polyester molded sheet. Available in .032" - 2.00". Standard color - Buff. Meets Gov't Specs - LP-509, I-24768/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.87 g/ccASTM D572
Water Absorption 0.60 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 46
Tensile Strength, Ultimate 69.0 MPa
Flexural Strength 159 MPa
Flexural Modulus 6.90 GPa
Compressive Strength 207 MPa
Shear Strength 97.0 MPaASTM D732
Izod Impact, Notched 4.30 J/cmedgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.3
@Frequency 1e+6 Hz
ASTM D150
 4.8
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 1.59 mm
Perpendicular, Short Time in Oil and Air; ASTM D149
Dissipation Factor 0.011
@Frequency 1e+6 Hz
ASTM D150
 0.015
@Frequency 60 Hz
ASTM D150
Arc Resistance 150 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CApproximate temperature class

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3)
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
Haysite 46000 Polyester SMC, 30% Glass Reinforced

PHAY14 / 45620

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.