Description: Dielectric grade that provides superior electrical and moisture resistance. Encapsulates semiconductor devices requiring very high purity and optimum moisture performance. Candidate for chip-on-board applications, excellent adhesion characteristics. Applications: Hybrids, and mica capacitors. Information provided by Cosmic Plastics Inc |