MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SHIELD® 4900 Conductive Coating
Categories: Polymer; Adhesive; Thermoset

Material Notes: CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Filler systems include nickel, silver, silver-copper, or nickel-silver blends.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 - 1.65 g/cc1.35 - 1.65 g/cc
Volatile Organic Compounds (VOC) Content 731 g/l731 g/lBulk
Thickness 25.4 microns1.00 milRecommended
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.050 ohm<= 0.050 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Shelf Life 6.00 Month6.00 MonthSpray
 9.00 Month9.00 MonthBulk
 
Descriptive Properties
BinderAcrylic
ConsistencyThin Fluid
Coverage34 ft2/lb
FillerAg
Mix Ratio1-part
Spraying Viscosity, #2 Zahn Cup19 - 22 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME166 / 28388

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.