MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics T-Wings Heat Spreaders
Categories: Other Engineering Material

Material Notes: Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreaders consist of 5oz. [0.007inch/0.18mm thick] flexible copper foil between electrically insulating films. High strength silicone PSA (pressure-sensitive adhesive) provides a strong bond to the component. The compliant nature of these “thermal wing” heat spreaders permits nearly 100% adhesive contact with non-flat package surfaces, optimizing thermal and mechanical performance.

Features/Benefits: Component junction temperature reduction of 10-20°C is common, Easily added to existing designs to lower component temperatures and improve reliability, Custom shapes available for complex designs, Low profile [0.33mm/0.013in] allows use in limited space environments, Easy peel and stick adhesion to all surfaces, including packages with residual silicone mold release, Offers low cost cooling for many package types, Low application force (<5psi/0.03MPa) minimizes risk of damage to component, Wide range of standard sizes, Pliable nature allows conformance to concave or otherwise non-flast surfaces for optimal thermal and mechanical performance, Light weight (0.039 oz/inch2), Standard parts are scored for easy forming and alignment, Easy removal for device replacement and Available die-cut on continuous rolls

Typical Applications: Microprocessors, Memory modules, Laptop PC’s and other high density, hand held portable electronics, and High speed disk drives.

RoHS compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 25.0 micronsInsulator Layer
 50.0 micronsPSA Thickness; Visual
 178 micronsThermal Conductor
 330 micronsTotal; ASTM D374
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 0.0230 MPa
@Temperature 100 °C,
Time 3600 sec
Lap; ASTM D1000
 0.414 MPa
@Temperature 25.0 °C,
Time 3600 sec
Lap; ASTM D1000
Peel Strength 0.216 kN/m60 min, 100°C, ASTM B571/D2861
 0.432 kN/m1 min, 25°C, ASTM B571/D2861
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 200 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthChomerics
 
Descriptive Properties
ColorBlack
Creep Adhesion135°C, 3kPa, on aluminum, P.S.T.C. No. 7
Insulator TypeBlack Polyester
Pressure-Sensitive Adhesive TypeSilicone based
Thermal ConductorCopper
Weight, oz/inch20.039

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating

PCHOME201 / 130911

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.