MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese 280 LDPE polymer for adhesives and molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: 280 resin is designed for extrusion and molding applications, and is also well suited for compound and masterbatch applications. It may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1520 - Olefin polymers, and its specifications 2.2, subject to extraction limitations on the finished food-contact article as specified in that regulation. Additives: None

Applications: Adhesives & Sealants; Compounds & Masterbatches; Molding & Miscellaneous

Information provided by Celanese Corporation.

Key Words: extrusion and molding applications and is also well suited for compound and masterbatch applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccAT Plastics PTM-03
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Hardness, Shore D 47ASTM D2240
Tensile Strength at Break 7.00 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 220 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 0.190 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 104.5 °CDSC; ASTM D3417
Vicat Softening Point 87.0 °CASTM D1525
Brittleness Temperature -25.0 °CASTM D746
Ring & Ball Softening Point 130 °CASTM E28
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA206000 Low Density Polyethylene
Borealis CA9150 Low Density Polyethylene
Celanese 191A LDPE polymer for adhesives, automotive and compounds
Celanese 193 LDPE polymer for adhesives, automotive and compounds
Borealis CA8200 Low Density Polyethylene

PATEVB22 / 25978

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.