MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SHIELD® 2054 Conductive Coating
Categories: Polymer; Adhesive; Thermoset

Material Notes: CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used for electronic enclosures.

Application: With their excellent leveling and uniformity, these coatings are compatible with all commercially available application technologies, including high volume/low pressure (HVLP) spray systems, and conventional propeller-agitated pressure pots. As low-settling compounds, they are ready for use after simple mixing in a paint shaker. They are supplied ready-to-spray, and don’t required additional thinning, although MEK can be used.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 - 1.60 g/cc
Volatile Organic Compounds (VOC) Content 75 g/l
Brookfield Viscosity 1200 - 1600 cP100 rpm. spindle #3 @ 25°C; Suggested Spraying Viscosity #2 Zahn Cup
Thickness 38.0 micronsRecommended
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.030 ohm
@Thickness 0.0381 mm
Shielding Effectiveness 75 dBminus water
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 75.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 24.0 °C
followed by 30 min @ 65°-85°C
 24.0 hour
@Temperature 24.0 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ConsistencyThin Fluid
Coverage10.4 m2/liter0.025 mm thick
FillerSilver plated Copper
Mix1-part
PolymerWater-based acrylic/urethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME139 / 28361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.