Hostacom X M2 T12 356036 is a 21% talc filled PP homopolymer, with high flowability, high stiffness, low odor and high thermal resistance. Product is available as non color matched, black, pellet form. This grade is delivered in 356036 color version.Information provided by LyondellBasell. |