MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® G-952 Fluoroelastomer Terpolymer, 69% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-952 is a terpolymer suitable for various peroxide cure systems. DAI-EL® G-952 can be formulated to eliminate the post cure process. DAI-EL® G-952 is suitable for transfer and compression molding applications requiring excellent chemical and steam resistance. DAI-EL® G-952 has better low temperature resistance than high fluorine terpolymers such as G-901 and G-902.

Typical Applications: O-Rings, gaskets, seals, tubing

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.89 g/cc1.89 g/cc
Mooney Viscosity 40
@Temperature 121 °C
40
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373
 73
@Treatment Temp. 232 °C,
Time 252000 sec
73
@Treatment Temp. 450 °F,
Time 70.0 hour
Air Oven Aging
Tensile Strength at Break 25.1 MPa3640 psi
 22.6 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
3280 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
Elongation at Break 320 %320 %
 307 %
@Treatment Temp. 200 °C,
Time 252000 sec
307 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
100% Modulus 4.80 MPa
@Strain 100 %
696 psi
@Strain 100 %
Compression Set 24 %
@Temperature 200 °C,
Time 252000 sec
24 %
@Temperature 392 °F,
Time 70.0 hour
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -14.0 °C6.80 °FLow Temperature Retraction, TR10
Brittleness Temperature -26.0 °C-14.8 °FEmbrittlement
 
Processing PropertiesMetricEnglishComments
Cure Time 0.800 min0.0133 hourts2, scorch time
 1.10 min0.0183 hourt'50, time to 50% cure
 1.60 min0.0267 hourt'90, time to 90% cure
 10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
Press Cure
 240 min
@Temperature 200 °C
4.00 hour
@Temperature 392 °F
Post cure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 69 %69 %
 
Descriptive Properties
ColorWhite to light pink
MH29.6 dNmmaximum torque
ML0.5 dNmminimum torque
Test Formula100 phrDAI-EL® G-952
 3 phrPeroxide (50% Activity)
 3 phrZinc Oxide
 30 phrMT Carbon Black (N-990)
 4 phrTAIC (72% Activity)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin DAI-EL® Perfluor GA-500 Perfluoroelastomer

PDAIJ9860 / 209931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.