MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1060 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Product Description: StarCLEAR CLR-1060 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market.

Features:
Soft Touch
Rubbery Feel
Excellent Colorability
Excellent Clarity

Processing Method: Injection Molding

Information Provided by STAR Thermoplastic Elastomers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Viscosity 16300 cP
@Shear Rate 10994 1/s,
Temperature 210 °C
16300 cP
@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 59
@Time 10.0 sec
59
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 4.67 MPa
@Time 7200 sec
677 psi
@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 700 %
@Time 7200 sec
700 %
@Time 2.00 hour
Die C; ASTM D412
300% Modulus 2.73 MPa
@Time 7200 sec,
Strain 300 %
396 psi
@Time 2.00 hour,
Strain 300 %
Die C; ASTM D412
Tear Strength 29.8 kN/m170 pliASTM D624
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Clear, but thickness not quantified
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7030-1000 TPE

PSTAQ959 / 131268

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.