MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chang Chun Plastic PBT2100 Fire Retardant PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Information provided by Dowell Trading Company Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 - 1.44 g/ccASTM D792
Water Absorption 0.050 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.013 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88ASTM D785
Tensile Strength, Ultimate 50.0 - 70.0 MPaASTM D638
Elongation at Break 4.0 - 6.0 %ASTM D638
Flexural Yield Strength 90.0 - 120 MPaASTM D790
Flexural Modulus 2.50 - 3.50 GPaASTM D790
Izod Impact, Notched 0.250 - 0.340 J/cm
@Thickness 6.35 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohmASTM D257
Dielectric Constant 3.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 225 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 165 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.7937 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chang Chun Plastic PBT1200M General Purpose PBT
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
BLUESTAR 201-G30202 PBT, 30% Glass Filled
BLUESTAR 201-G25202 PBT, 25% Glass Filled
BLUESTAR 201-G20202 PBT, 20% Glass Filled

PDOWELC33 / 30764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.