Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength. Main Characteristics: Very low viscosity and Good mold release Applications: VCD, Audio-CD, DC-ROM, CD-R, CD-RW, CD-RAM and DVD, DVD-R, DVD-RW CAS: 103598-77-2 Information provided by LG Chemical |