Properties: Cellulose acetate General Properties: Cellulose esters are thermoplastic resins partially produced using biomass like wood. Applications: Process: - Injection molding
- Plate extrusion
- Thermoforming
Markets: - Cosmetic / luxury
- Appearance parts
Properties:- Up to 63% biobased
- Non biodegradable
- Rigid
- Transparent
Information provided by NaturePlast Bioplastics Experts |