MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BJB Enterprises TC-854 A/B Rigid Polyurethane Casting System
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Rigid Polyurethane Polycarbonate-like

TC-854 is an extremely stiff, high impact, translucent material making it ideal when exact color matching is required. When coupled with the low viscosity, low shrink and high heat deflection temperature, this material is always a popular choice for a wide variety of applications. Features: RoHS/REACH compliant, Odorless, Translucent, High impact strength, Low viscosity, High heat distortion temperature, Excellent for hand, vacuum, or pressure casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccPart B
 1.17 g/ccPart A
Density 1.20 g/ccASTM D792-00
Brookfield Viscosity 165 cP
@Temperature 25.0 °C
Part A
 450 cP
@Temperature 25.0 °C
Mixed
 725 cP
@Temperature 25.0 °C
Part B
Linear Mold Shrinkage 0.0010 in/in12”x1/2”x1/2”
Storage Temperature 65.0 - 80.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82 - 86ASTM D2240-04e1
Tensile Strength 10060 psiASTM D638-03
Elongation at Break 10.5 %ASTM D638-03
Tensile Modulus 330000 psiASTM D638-03
Flexural Strength 13700 psiASTM D790-03
Flexural Modulus 360000 psiASTM D790-03
Izod Impact, Notched 1.14 ft-lb/inASTM D256-05
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 185 - 195 °FASTM D648-04
Deflection Temperature at 1.8 MPa (264 psi) 165 - 175 °FASTM D648-04
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 200 °FMax cure temp.
Cure Time 1.00 - 3.00 hour
@Temperature 25.0 °C
Step 1 recommended high temp cure (as tested).
 16.0 hour
@Temperature 82.2 °C
Step 2 recommended high temp cure (as tested).
 120 - 168 hour
@Temperature 25.0 °C
Optional low temp cure
Working Life 6.00 - 8.00 min
@Temperature 25.0 °C
100 g.
Gel Time 7.00 - 9.00 min
Shelf Life 6.00 MonthStored at recommended temperatures.
 
Descriptive Properties
Color / AppearanceColorlessPart B
 Pale YellowPart A
 Transparent Pale YellowCured
Demold Time (hrs)2 - 3@ 77°F
Mix Ratio by volume100 to 66Part A to Part B
Mix Ratio by weight100 to 60Part A to Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYT9907 / 287687

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.