MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ A-3 Bonding Agent, Primer and Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Adhesion promoter and primer for coatings, sealants and adhesives on metals, glass and ceramic.
  • Exceptional moisture and high pH resistance.
  • Outstanding harsh environment protection and cathodic corrosion protection when used with the B-4811.

Applications: Exceptional corrosion and chemical protection. Promotes adhesion and provides primer protection on most metals, ceramic and glass (including sapphire), most elastomers (including silicon) and low surface energy substrates. Functional for a wide range of overmold materials, paints, coatings, encapsulates. High thermal stability (250°C) and chemical resistance. Suitable for bonding semiconductor material. Used as adhesive for very thin bond lines (½ mil) such as for glass-to-glass and glass-to-polyethylene bonding. Compatible for use with BONDiT B-4X epoxy series. Ambient cure 60 min or accelerated thermal cure. Water white to slight amber.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.018 - 1.038 g/ccASTM D1298
Viscosity Measurement 4.5 - 8.5ASTM D445
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 392 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.442 - 1.448ASTM D1218
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 150 °C
 
Descriptive Properties
ColorClear with stray color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2110817D5 Conductive Silver Polymer Paste
SunChemical Gwent R2070613P2 Resin Binder
SunChemical Gwent D2070209P6 White Dielectric Paste
SunChemical Gwent D2020409D8 Dielectric for Stainless Steel
SunChemical Gwent C2110127D3 Nanocopper based Paste

PAQREL11 / 24227

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.