MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for applications subject to impacts and rough handling. QC-8800 is also suggested for applications requiring excellent fatigue resistance. Form and Color = Rolled sheet, Black. Glass Fiber Length = 1 inch.

A. Schulman has acquired Quantum Composites.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccASTM D792
Water Absorption 0.10 %24 Hrs. ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 70ASTM D2583
Tensile Strength, Ultimate 344 MPaASTM D638
Tensile Modulus 26.1 GPaASTM D638
Flexural Yield Strength 585 MPaASTM D790
Flexural Modulus 20.6 GPaASTM D790
Compressive Yield Strength 289 MPaASTM D695
Compressive Modulus 18.6 GPaASTM D695
Izod Impact, Notched 19.2 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cmASTM D257
Dielectric Strength 12.0 kV/mmASTM D149
Arc Resistance 129 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature 20.0 °C
TMA
Maximum Service Temperature, Air 260 °CDeflection Temp; Load not reported; ASTM D648
Shrinkage 0.00 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 132 - 149 °CMold temperature
Shelf Life 2.00 Month
@Temperature 23.9 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
A. Schulman BMC 845 30% Glass Filled Vinyl Ester
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled

PCOQCA / 29047

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.