MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT AS1621 RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Oxime cure products which are solvent free. It exhibits good primerless adhesion to many substrates especially plastics and cures rapidly at room temperature when in contact with atmospheric moisture. This product can be described as low corrosive but would not be recommended for use with copper or its associated alloys.

Key Features

  • Excellent flow and self leveling properties
  • Low corrosion
  • Good adhesion to substrates
Application: Applications include but are not limited to screen printed gaskets automotive

Cured Product: 7 days at 23+/-2°C and 50+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³BS ISO 2781
Brookfield Viscosity 24000 cP24000 cPMixed
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2424ASTM D2240-95
Tensile Strength 2.00 MPa290 psiISO 37
Elongation at Break 410 %410 %ISO 37
Tensile Modulus 0.000558 GPa0.0810 ksiYoung's
100% Modulus 0.359 MPa52.0 psi
Tear Strength 3.33 kN/m19.0 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D-257
Dielectric Constant 2.62.6ASTM D-150
Dielectric Strength >= 18.0 kV/mm>= 457 kV/inASTM D-149
Dissipation Factor 0.00100.0010ASTM D-150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 306 µm/m-°C170 µin/in-°F
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 230 °C446 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 19.0 min0.317 hourTack Free Time / Skin Formation
 <= 1440 min
@Temperature 23.0 °C
<= 24.0 hour
@Temperature 73.4 °F
3mm Depth
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorWhite
Cure typeOxime
RheologyFlowable
Volume Coefficient of Thermal Expansion920 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL017 / 314500

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.