MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
A. Schulman BMC A50-MS General Purpose Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compression molding of intricate parts. Typical applications are appliance bodies, insulators, bobbins and electrical connectors.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.83 - 2.03 g/ccMolded
Linear Mold Shrinkage 0.0025 - 0.0030 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 40
Tensile Strength 6900 - 8900 psi
Flexural Strength 14500 - 18500 psi
Flexural Modulus 1200 - 1400 ksi
Compressive Strength 19500 - 23500 psi
Izod Impact, Notched 5.00 - 7.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 365 - 415 V/milshort time
Arc Resistance >= 191 sec
Comparative Tracking Index >= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
IDI Composites Rosite® 3550F BMC Thermoset Polyester, 30% Glass Reinforced
Emerald Performance Materials EPALLOY® 8330 A85 Epoxy Phenol Novolac Solution
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade

PBMC921 / 123385

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.