MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer PP-RP340R Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: PP RP340R is a nucleated polypropylene random copolymer with medium fluidity and outstanding transparency and gloss and is designed for injection molding applications. ?RP340R? is the material of choice for applications where transparency is a primary requirement. This grade is also suitable for injection stretch blow molded containers and bottles. This product combines good see through clarity and excellent moisture barrier properties with hot fallibility. Therefore, ?RP340R? offers an effective alternative for PET and PVC for the packaging of non-oxygen sensitive products such as confectionary, herbs, toiletries and cosmetics.

Processing Method: Injection molding, Injection stretch blow molding.

Features: High melt flow, Excellent transparency, High gloss, Random copolymer.

Typical Applications: Household containers, housewares - Packaging for food, cosmetics and pharmaceutical products Clear tubs and pots for ice cream, yoghurt and other desserts -Medical sector such as syringes, test tubes and vials, Lids, caps and closures, CD and DVD boxes, Sports, Leisure and toys.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 1050 MPaASTM D790
Izod Impact, Notched 65.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CASTM D648
Vicat Softening Point 127 °C
@Load 1.02 kg
ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 22 %
@Thickness 1.00 mm
ASTM D1003
Gloss 73 %60°; ASTM D2457
 
Descriptive Properties
Accelerated Oven Aging360 hrsIn air @ 150°C. ASTM D3012

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI985 / 250389

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.