MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® 1900GF20 BK 2.7206 PPE, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: VESTORAN® 1900GF20 BK 2.7206 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO). As a material of amorphous structure VESTORAN® 1900GF20 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp. Moldings of VESTORAN® 1900GF20 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900GF20 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions. Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity. The even smaller shrinkage compared to non-reinforced VESTORAN® depends on the orientation of the glass fibers in the molded parts. VESTORAN® 1900GF20 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites by the Evonik Degussa GmbH-patented K&K process ("direct-bonding to rubber"). Compared to VESTORAN® 1900, VESTORAN® 1900GF20 offers higher rigidity and strength. Colored material contains only cadmium-free pigments.
Dry properties listed below
Industrial Sector: Automotive and Mobility
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water
Conformity: Automotive
Additives: Glass fibers
Processing: Profile extrusion, Sheet extrusion, K&K process
Special Characteristics: Amorphous, High heat resistant, Low warpage / Low shrinkage
Color: Black
Chemical Resistance: Acid resistance, Alkali resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Water Absorption 0.350 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00500 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00600 cm/cmISO 294-4, 2577
Melt Flow 24.0 g/10 min
@Load 21.6 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 106 MPaISO 527
Tensile Strength 110 MPaISO 527
Tensile Strength, Yield 110 MPaISO 527
Elongation at Break 3.00 %ISO 527
Elongation at Yield 2.80 %ISO 527
Tensile Modulus 5800 MPaISO 527
Flexural Modulus 5700 MPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
Tensile Impact Strength 260 kJ/m²NOTCHED; ISO 8256/1
Tensile Creep Modulus, 1 hour 5100 MPa
@Strain 0.500 %
ISO 899-1
Tensile Creep Modulus, 1000 hours 2300 MPa
@Strain 0.500 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohmRSD; IEC 62631-3-2
 1.00e+13 ohmsE; IEC 62631-3-2
Dielectric Constant 2.70
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 2.90
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 33.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
Dissipation Factor 0.000800
@Frequency 100 Hz
IEC 62631-2-1
 0.0180
@Frequency 1.00e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 175 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75-1/-2
Vicat Softening Point 193 °C
@Load 5.10 kg
50 K/h; ISO 306
 200 °C
@Load 1.02 kg
50 K/h; ISO 306
Glass Transition Temp, Tg 190 °CISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 0.800 mm
Oxygen Index 29.0 %ISO 4589-1/-2
 29.0 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 320 °CInjection Molding; ISO 294
 320 °C
Mold Temperature 80.0 °CInjection Molding; ISO 294
 80.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7943 / 325075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.