TRA-BOND 221U01 is an electrically insulating, non-sagging epoxy encapsulant formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and mechanical shock. The long work life and smooth consistency of TRA-BOND 221U01 make it ideal for use in automatic dispensers. We recommend storage at -40°C or colder. Information provided by Tra-Con Inc. |