System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Dow Fusabond® A560 Polymer Modifier
Categories:
Polymer
;
Thermoplastic
;
Adhesives, Sealants, and Coatings
Material Notes:
DuPont™ Fusabond® A560 is a chemically modified ethylene acrylate copolymer
Used as a polymer modifier
This former DuPont product line is now a Dow product line.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.930
g/cc
ASTM D792, ISO 1183
Melt Flow
5.6
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
Thermal Properties
Original Value
Comments
Melting Point
94.0
°C
ASTM D3418, ISO 3146
Processing Properties
Original Value
Comments
Processing Temperature
<=
310
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow Fusabond® N416 Polymer Modifier
Dow Fusabond® C190 Polymer Modifier
Dow Fusabond® C250 Polymer Modifier
Dow Fusabond® N493 Polymer Modifier
Dow Fusabond® P353 Polymer Modifier
PDTA4966 / 170406
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.